Horizontal striation control of cold rolled steel plate
Surface striated defects are important indicators affecting the surface quality of cold-rolled products . It is very difficult to solve the problem of surface ridges in many cold rolling mills in China, especially galvanizing units and continuous retreating units. The cause and solution of surface grain defects are an important part of the development of high-end cold-rolled product production technology. How is the surface grain pattern formed? When the strip is subjected to a sudden transition from the elastic zone to the plastic zone by the stress exceeding the yield limit, due to the effect of the yielding platform, unevenness and local flow deformation will occur on the strip section, and the surface yielding transverse stripes will occur. The microscopic cause is due to the "nail anchor" effect of the Kodak air mass. When the solute atoms interact elastically with dislocations, they eccentrically gather around the dislocations to form a so-called "Kod's a...